Hello guys I am new here. Congrats to all of you for the great work.I am using carbon fiber pre-preg that cures for 2 hours at 175 degrees . Is it possible to cure at 50 degrees for much more time ?
Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Additional to what hanaldo said, it is almost certain that you will get a very bad surface, as the resin will never reach a low viscosity to give a nice finish.