|
Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Possibly, but sort of impossible for us to tell you that as it depends on your specific material. If 50 degrees is enough to activate the resin, then it should be able to cure after a sufficient amount of time and just achieve a much lower Tg. However, if it isn't enough to activate the resin, then it obviously won't cure.
The only way to know is either to try it yourself and conduct a series of tests, or to contact the manufacturer and speak to a technician. Else, if you can tell us what specific material you are using then someone here might have experience with it and may be able to guide you a bit better.
|