You really want to get the oven heating evenly, as even though there isn't any real problem in baking the part for longer; the uneven curing will lead to stresses and warping.
A shrouded oven fan is the best solution, and if the part is really long then you may need to look at a number of elements/fans to get the whole oven heating evenly.
|