Hi, I purchased 3 different types of bagging material from you a couple of years ago, now I can't identify what their specific application is cause your product codes have changed. What I have is VBF152 (blue), VBFEL (green), VBRF (green). Can you clarify?  I noticed the VBFEL is probably 'elastic', it however sticks firmly to the prepress after curing....Thanks for helping Alexander





Reply
Warren (Staff)
Warren (Staff)
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Some of the colours don;t seem to match.  VBF152 was our standard vacuum bagging film which is a 1.52m wide lay flat tube.  You can tell the elastifilm apart from it is it has a semi-gloss finish, is a slightly different shade of green and is NOT a lay flat tube - plus it feels a lot more stretchy.  The Elastifilm does not have good release properties.  Our older release films were available in perforated or unperforated and both were blue.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search