When sanding, to get to a high gloss, work your way up the grits to 1200-1500 and then you should be able to polish the resin back to a high gloss.
GlassCast 3 can be used on flooring to give a high gloss finish. You can also use epoxy compatible pigments if you so wish.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|