By Pmwoods - 3/22/2018 4:28:41 PM
Hi,
In first sorry for my English, i'm french...  I have a project for a dinner table in wood and epoxy. Two lumber with an epoxy river in the center. For this operation i think Glasscast 50 is the best. But i want to cover all the table with epoxy and for this operation, i don't know which product must i use glasscast 3 or another ?
Another question will come later...
Thanks for your answer Regards from frogs
|
By Warren (Staff) - 4/26/2018 4:35:54 PM
For thicker work like encapsulating lego you definitely want GlassCast 50.
I did a lego table with the original GlassCast 3 in many layers (before we had GlassCast 50 - which is what i would use now) and you find some parts are very hard to not get trapped air, even if you use a heat gun or blow torch. I even used cocktail sticks to try and burst some bubbles. Despite that it still looked great as these photos show:




|
|