Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Bonding a Glassfibre polyester component to a wooden structure
Bonding a Glassfibre polyester component to a wooden structure
Post Reply
Like
2
Bonding a Glassfibre polyester component to a wooden structure
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Neale Lee
Neale Lee
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 4
What type of adhesive should I use to bond a glassfibre / Polyester component to a wooden structure?
Reply
Like
2
Hanaldo
Hanaldo
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
An epoxy adhesive would be my choice, though polyurethane would bond well too. Both are quite easy to bond to, just prep the surfaces well.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search