By Neale Lee - 3/15/2018 12:22:34 PM

What type of adhesive should I use to bond a glassfibre / Polyester component to a wooden structure?
By Hanaldo - 3/16/2018 2:04:37 AM

An epoxy adhesive would be my choice, though polyurethane would bond well too. Both are quite easy to bond to, just prep the surfaces well.