GC50 Epoxy does not stick to EL160 High Temp Laminating Resin ! What now?


GC50 Epoxy does not stick to EL160 High Temp Laminating Resin ! What now?
Author
Message
geedee
g
Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)
Group: Forum Members
Posts: 3, Visits: 11
Hi All,

I'm a beginner in Composite World.

I created a mould from a bonnet from a reacecar.


So far, so good.

Next step was to create a carbon fibre bonnet.
First I used several coats of easy lease Chemical Release agent on the mould.
Then, I did one layer of GC50 Epoxy Compatible Gelcoat. I used 2% MEKP hardener, maybe a little more.
Then, I did One layer of 200gr Carbon Fibre, 2mm Lantor Soric core material, and then again a layer of 200gr Carbon Fibre.



Next was all necessary thing for vacuum bagging., as shown below;.



The day after I removed the peel ply, and took the bonnet out of the mould.



But then I saw the GC50 did not stick to the EL160 resin. I could peel it all off !!



Which resulted in this on the floor !







this leave me with a bonnet with a very wavy surface !





Question1 : What did I do wrong?
Question2 : How can I repair this?

Thanks,

Gerry.

Reply
geedee
g
Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)
Group: Forum Members
Posts: 3, Visits: 11

For anybody who wants to know how it turned out : Is was OK.

See this google photoalbum for the full story so far.

Thanks Easy Composites, thanks Warren.

Gerry.

Edited 7 Years Ago by geedee
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search