By geedee - 2/25/2018 10:24:09 PM
Hi All,
I'm a beginner in Composite World.
I created a mould from a bonnet from a reacecar.
 So far, so good.
Next step was to create a carbon fibre bonnet. First I used several coats of easy lease Chemical Release agent on the mould. Then, I did one layer of GC50 Epoxy Compatible Gelcoat. I used 2% MEKP hardener, maybe a little more. Then, I did One layer of 200gr Carbon Fibre, 2mm Lantor Soric core material, and then again a layer of 200gr Carbon Fibre.

Next was all necessary thing for vacuum bagging., as shown below;.

The day after I removed the peel ply, and took the bonnet out of the mould.

But then I saw the GC50 did not stick to the EL160 resin. I could peel it all off !!

Which resulted in this on the floor !



this leave me with a bonnet with a very wavy surface !


Question1 : What did I do wrong? Question2 : How can I repair this?
Thanks,
Gerry.
|
By Warren (Staff) - 5/14/2018 4:16:10 PM
Hi GeeDee, glad it all turned out ok in the end.
|
|