	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            Hi Nicola,
  Flax can be used  in just the same fashion, cutting it to strips to laminate it where you need it.  It wets out relatively easily and its relatively soft and pliable nature means it can be made to conform to most mould shapes.  From a mechanical perspective, flax is not as stiff as a similar weight woven glass cloth, so you may find when replacing glass with flax, you need additional layers.                 
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |