Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
For our UD, the support netting is a polyester yarn which has a melting point of 295C. I am not aware of any other UD's with a specific higher melting point for the support netting. Commonly the support netting tends to be a woven material such as polyester or a thermoplastic such as polypropylene. Both would not have the raw heat resistance you require.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|