By shazhao - 1/12/2018 5:27:42 AM
I wish to know is there any UD carbon fabric that its binders can sustain a temperature of 400 to 600 ℃, I wish to buy some if there is such a product.
|
By Warren (Staff) - 1/12/2018 9:48:55 AM
For our UD, the support netting is a polyester yarn which has a melting point of 295C. I am not aware of any other UD's with a specific higher melting point for the support netting. Commonly the support netting tends to be a woven material such as polyester or a thermoplastic such as polypropylene. Both would not have the raw heat resistance you require.
|
|