Friends, please guide me I am new in this field, Which type of carbon fiber fabrics can be used for making automotive parts. What is the difference in it?  

 

Rakesh Verma
+8613861177443
vermachina@gmail.com



Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Basically pretty much any fabric can be used.  Typically people tend to use a 2/2 Twill 3k around 200gsm



Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search