By vermachina - 12/27/2017 6:31:09 AM
Friends, please guide me I am new in this field, Which type of carbon fiber fabrics can be used for making automotive parts. What is the difference in it?
|
By Warren (Staff) - 1/2/2018 9:03:06 AM
Basically pretty much any fabric can be used. Typically people tend to use a 2/2 Twill 3k around 200gsm
|
|