I've spent about the last week researching resin's for a very high heat application with little success.  Highest temp range I've seen is approx 600-700*f.   Any suggestions on brands, or otherwise would be appreciated.  The project is an exhaust pipe with the header section (first 12" or so) reaching up to 1100* for brief durations of 2-5 seconds.

Second thought, I've also reached out to several chemical manufacturers for heat reflective coatings, however dead end there too.  

Third idea, cf skin a steel section where exposed to the extreme heat, but would the bond with the steel still seep into the resin and soften or fail?
Reply
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Have a look over at this website they may be able to help you out.

http://www.sstubetechnology.com/ceramic-matrix-composites/

http://www.sstubetechnology.com/integrated-heat-shields/

Otherwise you will have to look at a metallic heat shield and try and wrap it but as above most thermosets dont like high temps so you may need to look at thermoplastics?