Hi All,

         Just a query about a carbon fibre section of my mountain bike frame that has a crack on it, would the repair resin be suitable? I've attatched a photo, hope it helps.

Many thanks in advance

Ian Todd
Attachments
P10102142.jpg (650 views, 659.00 KB)
Reply
Iant
Iant
Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)
Group: Forum Members
Posts: 4, Visits: 16
Hi Matt,

            Once again thanks. That seems very acceptable think i could get away with up to 0.3 or 0.4. So will be ordering the kit this weekend.

Many many thanks for your advice.

Ian Todd