By Iant - 7/31/2012 11:10:10 PM
Hi All,
Just a query about a carbon fibre section of my mountain bike frame that has a crack on it, would the repair resin be suitable? I've attatched a photo, hope it helps.
Many thanks in advance
Ian Todd
|
By Iant - 8/1/2012 2:09:00 PM
Hi Matt,
Once again thanks. That seems very acceptable think i could get away with up to 0.3 or 0.4. So will be ordering the kit this weekend.
Many many thanks for your advice.