Hello folks. 

I'm fairly new to the composites game, having only really used epoxies to create glassy finishes on work surfaces so far. 

I'm currently making some prototypes, and want to create a piece of cast resin which will diffuse light similarly to commercially available polycarbonate diffusing sheets. 

I'm hoping to use standard casting resin, a silicon mould/other form and an additive. 
I've read that there are silicon-based products that may be able to achieve this effect, but haven't been able to ascertain if this is the case or what I'd need to use. 

Any help appreciated! 

Cheers, 

Ren 


Edited 9 Years Ago by Warren (Staff)
David Vale
D
Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)Supreme Being (160 reputation)
Group: Forum Members
Posts: 10, Visits: 109
I would like this too, an aircraft panel that is highly glossy and reflective is not good. At the moment my only solution is a matt lacquer to go on top of that lovely glossy finish!!

Retired - Thank heavens, and still don't have enough time during the day
Warren (Staff)
Warren (Staff)
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You could try experimenting with opaque pigments.  Added in very small quantities I would expect you to gradually go from a tint all the way to opaque with a middle ground where the light still shines through but is diffused somewhat by the pigment so is not really translucent.

Might take a bit of experimenting to find the sweet spot and see if you would get an even appearance.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search