Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
The 10mbar figure is based on sea level and standard atmospheric pressure ie 1 bar/1000mbar, so the higher you go, the less force is applied against the bag, so realistically with a very high vacuum pump, for exmple 0.03mbar, then as you approach 900meters or 900mbar atmospheric (eg a lower altitude in a severe "low pressure" weather storm), then the level of force applied to the vacuum bag and hence the pre-preg may well not be enough to ensure a pin hole free finish without extra force being applied, such as in a press or an autoclave.
However this is quite a rare scenario for most users.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|