Hi all, I'm sure this has been covered somewhere in the forum but I kept getting sidetracked while looking and was taken ages.

I have completed my uni mould and really happy with the results. 1 small repair needed. I am planning eventulally producing my final part from cf using infusion but for now want to make one using polyester gellcoat and reinforced with csm. Mainly due to cost with Christmas coming. That will be one in the new year.

Can I use chemical release agent multiple coats then the polyester gellcoat and reinforcement it will be 2x 200g csm then 3x 300g csm. The reason I ask is that someone told me you could only use 2 layers of 200g csm for the first pull and that chemical release agent wouldn't be good for the first one.

Thanks in advance

Phil
Reply
Phil_123
Phil_123
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 5, Visits: 169
That's great Matt thanks.

I really like the Easy-Lease. The plug came out of the mould so easy.