Hi,

I have just made a plug to make a mould from.

In finalising the plug I will place several layers of easylease on it, followed by several layers of wax (polished).

My question is this;

Would the polyester based body filler used in making the mould affect the tooling gel coat?

Thanks in advance
Reply
neilb
neilb
Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)Supreme Being (763 reputation)
Group: Forum Members
Posts: 107, Visits: 503
2k primer is available in rattle cans, obviously health and safety goes without saying, wear a mask, have as little bare skin showing as poss, well ventilated area