Hi,

I have just made a plug to make a mould from.

In finalising the plug I will place several layers of easylease on it, followed by several layers of wax (polished).

My question is this;

Would the polyester based body filler used in making the mould affect the tooling gel coat?

Thanks in advance
By neilb - 8/1/2012 1:46:03 PM

Bonobo (31/07/2012)
not really it says on the data sheet, second line ''excellent 1k primer'' you want something like this http://www.specialistpaints.com/products/2k-primer-canz

it has a sealed body inside the can containing the activator, attach a ring to a pin protruding the base and twist puncturing the container inside to mix the contents. you'll have to do some detective work to find a supplier in your location