Yeah .. I never wet sand between XCR coats, .. no need to wet sand .. I just sand with 240 dry .. and it is very important not to sand through to the fabric ...
I have used several other Coating resins, including West Systems and EC's "old" Coating Epoxy, none of the others have come close to XCR for ease of use and quality of the finished product. I even use it as "clear coat" because it is so easy to flat and get a "satin Matte" finish.