Hi guys!

I need a bit of help from you in order to be able to do something worth showing here jejej.

Well, the thing is that I have a perfect piece as a mould but is made out of wood. Is there any problem of using the chemical easy release product or should I first coat the piece of wood with something?

Thank you very much in advance
oekmont
oekmont
Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
In my early composites days I have done it several times without coating, but with a wax type release agent. It worked (not that great, but it did the job) with polyester molds, but I guess it will not with epoxy tooling resins, as epoxy has much better bonding propertys.

Nowadays  I would always use a light clearcoat, before tooling.

MarcosTG
M
Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)
Group: Forum Members
Posts: 15, Visits: 62
Thanks for your answer Oekmon,

Which clear coat do you suggest? Polyurethane?

Chheers
oekmont
oekmont
Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Polyurethane would be my choice. But as long as it is 2k it will be fine.

MarcosTG
M
Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)Supreme Being (204 reputation)
Group: Forum Members
Posts: 15, Visits: 62
oekmont - 10/18/2017 8:23:31 AM
Polyurethane would be my choice. But as long as it is 2k it will be fine.

Do you mean the fabric type by 2k?

oekmont
oekmont
Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
No, sorry. I meant 2 component lacquer. I didn't translate that.