Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Typically it only goes white when not fully cured as uncured epoxy is hydroscopic. Maybe you need more time and a warm place to fully harden the resin. Also if your mix ratio is slightly out, the resin can seem hard but remain vulnerable to moisture absorption due to the incorrect balance of hardener and epoxy leaving uncured material in the hard resin mix.
Get the parts somewhere nice and warm to help drive out as much moisture as possible.