Group: Forum Members
Posts: 90,
Visits: 634
|
Hey. When any of the xcr resin comes in contact with water it goes white.. Even after 3 or 4 days to cure.. Sanding removes it but it goes into the weave and is visable after another coat of resin, some.does go away but alot of it dosnt.any suggestions?
If you dry sand how are you to clean the part after?