You are correct, most infusion resins are capable, and perfectly fine with a room temperature cure. However, an elevated temperature post cure can have benefits in mechanical performance as well as the more obvious HDT. Rather than saying to cure at 110C, I would recommend you check for the correct post cure procedure for the resin system you are using.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|