Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pre-Pregs
»
Flow / cure temperature
Flow / cure temperature
Post Reply
Like
2
Flow / cure temperature
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Carbonphoenix
Carbonphoenix
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 12,
Visits: 134
Hey guys
I have started testing some bits using your prepreg and under a -1bar vac bag, I then put this into the oven and have tried both 100 and 110c for around 8hrs.
When I come to remove the part, it feels like it has cured, but is very dry to feel.
So I am a little concerned that my oven is going from ambient temperature to the 100 too quickly, and there is not enough dwell time at the flow stage (hope that's right terminology)
Therefore, I am trying to find what is the flow temperature for your surface and backing prepreg layers, so I can look to programme my PID to dwell for longer at that temp before moving into the cure.
Any ramp, dwell times and temperature ideas are very much appreciated, otherwise I will just sell carbon cheese graters.
Kind regards
Dave
Reply
Like
2
Reply
Carbonphoenix
Carbonphoenix
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 12,
Visits: 134
Excellent, thanks guys, I think that will give me enough to work with.
I just need to get my head around my PID (omega cn7800) to program this correctly
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Flow / cure temperature
Carbonphoenix
-
8 Years Ago
50 degrees for 1 hour, 60 degrees for 1 hour, 70 degrees for 1 hour. Then go to your final cure temp...
Hanaldo
-
8 Years Ago
70C is the temperature where the resin begins to flow. If you skip through this stage too quickly...
Warren (Staff)
-
8 Years Ago
Excellent, thanks guys, I think that will give me enough to work with. I just need to get my head...
Carbonphoenix
-
8 Years Ago
Same PID I'm using. It works really really well once you get it figured out. Just a little tip...
Hanaldo
-
8 Years Ago
Thanks Hanaldo, I will take your advice. Pleased the PID is a good one, just understanding how to...
Carbonphoenix
-
8 Years Ago
Yeh I know, I thought the same thing when I first started playing around with it. Omega's...
Hanaldo
-
8 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search