	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            As said, braided sleeve is the best way.  It can be very hard to get the fabric to precisely meet in exactly the right place when using normal fabrics.  Also depending on the diameter of the fabric, even if you aligned it perfectly down the tube, you might find it will never align perfectly around the tube.                
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |