Hi all

I've been lurking on here for a while and have recently started making some parts for a project car.  I've started using resin infusion hoping to get a more uniform finish and like everybody (I guess) I occasionally get voids where I havent gotten my cloth in to the corners but I'm also getting surface voids along the edge of where I have used closed cell foam as a stiffener.





The above is 2 layers of 200g carbon, the stiffener then another 200g layer on the back, any advise on what I'm doing wrong would be appreciated.

Thanks
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
You could do the outer skin with a peel ply on the back, bond in the core then do the inner skin.  It would be a bit of a pain doing it in two passes but it'd stop this problem.