Duratec


Author
Message
Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
dose any one no if you can thin down duratec 
For spraying ? 
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Is Simon stocking it or does he also just order it in from ATL? 

It's a pity Simon doesn't talk to me (I can only imagine it's because I'm at Kirkside now), he does have a lot of great products that I would be interested in. 
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
He has 20l, I don't know where he gets it from.