Newbie problems


Author
Message
Rovinmosin
Rovinmosin
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 97
Hi guys, I have ran into this issue before and cant figure out why. Sometimes when I run a part it comes out great and other times it comes out like this. Is this a wet-out issue?

Hand-layed 3 layers of carbon then vacuum bagged
Thin epoxy resin (will do it with polyester resin too)

Any thoughts?
Attachments
20170417_144645_HDR.jpg (625 views, 4.00 MB)
Reply
Rovinmosin
Rovinmosin
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 97
ok I will, thank you Warren!