Hi guys, I have ran into this issue before and cant figure out why. Sometimes when I run a part it comes out great and other times it comes out like this. Is this a wet-out issue?
Hand-layed 3 layers of carbon then vacuum bagged Thin epoxy resin (will do it with polyester resin too)
Any thoughts?
|
By Rovinmosin - 4/18/2017 6:33:05 PM
ok I will, thank you Warren!
|
|