Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
New Member Introductions
»
Hello I'm new to composites
Hello I'm new to composites
Post Reply
Like
2
Hello I'm new to composites
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Splay
Splay
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 65
Good morning,
I am Wes and reside in Panama City Florida. I am soon to be 41 a Father of 2 boys and a step father of 1 girl. My wife and I have celebrated our 4th year of marriage and we're going strong. I am a huge car fan and have worked on my own cars since I was 16. I am currently working on trying to start my own business as an automotive customizer. I have don stereo upgrades, dash and door panel painting, headlight and taillight housing swaps and more. Now I am looking to actually do it professionally and want to be able to offer custom carbon fiber parts as well. I look forward to getting going and hope I can get help when needed to understand everything.
I do have 2 project vehicles that I think I will start making parts for once I can get everything in order. The one I will probably start on first is my 1982 Toyota Supra. Since it is in pieces already lol.
I do have a couple questions I would like to throw out there.
1) I see alot of CF hoods in the market place but alot of them I notice warp really bad once they get hot or yellow or the top coat peels really bad. Is this common or are they sub-par parts? I do not want my parts to be this way how would I keep this from happening? I am planning on starting with smaller parts than a hood to get the knowledge and practice before I do a hood. Like I am planning on doing the headlight covers of the supra first. They are not big and are mostly flat.
2) Is CF strong enough to use to make brackets? For example an alternator bracket?
3) I have seen people make valve covers out of CF but I wonder how they get them to stand up to the heat of the engine bay?
Thank you in advanced for any an all advice and assistance you all are willing to give.
Thank you for having me here,
Wes
Reply
Like
2
Reply
Splay
Splay
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 65
Hey
Davro,
Thank you very much. I am assuming you just have to prep the part like you would paint? With a really good wet sand? How does it hold up? I just want to make sure I put out there a product I would buy.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Hello I'm new to composites
Splay
-
8 Years Ago
Hi and welcome to the forum. The problem with many parts is they do not have enough heat resistance...
Warren (Staff)
-
8 Years Ago
Thank you very much Warren. When you say post cure are you speaking of baking it in an oven? I...
Splay
-
8 Years Ago
Hi Wes, Welcome to the forums. I use 2K clear coat on all my products mainly because I use epoxy...
davro
-
8 Years Ago
Hey Davro, Thank you very much. I am assuming you just have to prep the part like you would...
Splay
-
8 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search