What's the best cloth gor skinning?


Author
Message
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
Hi guys,  iv skinned quite a few pieces out of the 2m I originally ordered,  was wondering what people's thoughts wet on the best cloth to use?  In terms of wrap ability and looks.
Reply
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
I'd certainly recommend using the 240g twill fabric that EC and other places sell, as it is much more stable and less likely to distort when handled and laid down, due to its more closely woven construction. It also looks better, in my opinion, although a touch more expensive. 