Lewismotorsport
Lewismotorsport
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 32
hi guys I've been tasked with door cards moulded to the shape to suit a door and rollcage has anyone any ideas other than high density polyurethane foam?
Reply
Like
3
Reply
Interloper393
Interloper393
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 90,
Visits: 634
Maybe pop a few pics up of what you have and aiming for
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Door card moulding.
Lewismotorsport
-
8 Years Ago
Use old door card as a base
Interloper393
-
8 Years Ago
Old door card cut and shut around the cage is the best route to go. Some people like to keep the...
Warren (Staff)
-
8 Years Ago
thank you warren, thats what im hoping, however what do you put into the door card in the shape of...
Lewismotorsport
-
8 Years Ago
Plastic pipe?
Interloper393
-
8 Years Ago
Plastic pipe would work, but if it were me I would cover the cage tube in 5mm sheet wax and splash a...
Hanaldo
-
8 Years Ago
Maybe pop a few pics up of what you have and aiming for :)
Interloper393
-
8 Years Ago
brill idea! this one wont be made to exact as the customer has messaged me now saying hes made a...
Lewismotorsport
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search