Hi all,

I've joined the forum to seek some advice.

I have a carbon fibre bicycle frame which has sustained some damage to the top tube, see attached pics.

I came across easy composites whilst searching for epoxy resin to fill in the chips but not having experience with these materials I would like some advice. 

My plan was to key the chipped area and fill with resin then touch up the paint so I would also like to know what my options are regarding the type of paint to use.

Thanks,
Mark
Attachments
IMG_0020.JPG (261 views, 1.00 MB)
IMG_0021.JPG (254 views, 1.00 MB)
IMG_0023.JPG (252 views, 1.00 MB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search