hello,I skinned parts just like the video of easycomposites,it is better to post cure one time at the end of the project or I must post cure the first layer of epoxy which is applied to do the trimming?

if I key the surface to the next layers and post cure at the end of the project do I have problems for delamination because the layers doesn't post cure individualy?
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You are best to post cure after the last layer of resin has been applied and cured, but NOT sanded smooth.  You would likely get some movement and sinking of the resin during a post cure, so it is best done before the final sanding smooth.  Once postcured, you can sand smooth and polish back to a gloss as normal.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search