Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Keying up still required after use of peel ply?
Keying up still required after use of peel ply?
Post Reply
Like
3
Keying up still required after use of peel ply?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Willi1991
Willi1991
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 16,
Visits: 32
There are different schools of thought when it comes to this and I thought I'd put it to the group. I've heard people say that if peel ply is used there is no need to key the area up before laminating/painting/glueing. I've also heard the opposite that even if you have peel plyed once the laminate is no longer 'green' use must key up before adhering to it.
Thoughts?
Reply
Like
3
Reply
scottracing
scottracing
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
I will always abrade after using peel ply then a bit of acetone to clean up prior to bonding
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Keying up still required after use of peel ply?
Willi1991
-
8 Years Ago
I will always abrade after using peel ply then a bit of acetone to clean up prior to bonding
scottracing
-
8 Years Ago
Keying up is a lot quicker on a peel ply finish as half the roughness is already there so there is...
Warren (Staff)
-
8 Years Ago
I understand it's along quicker but is it necessary. Was peel ply designed to completely irradiate...
Willi1991
-
8 Years Ago
Peel ply is designed primarily as a removable pourous barrier between the laminate and other part of...
Warren (Staff)
-
8 Years Ago
Thank you for the clarification. Very useful information. Cheers
Willi1991
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search