Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Peel ply is designed primarily as a removable pourous barrier between the laminate and other part of the bagging stack. Providing a good surface for secondary bonding is a secondary function and in essence a byproduct of the peel ply's surface texture. In most cases, the peel ply finish will be fine, however a good key of the surface may well give slightly better results. Also be aware that there are some "release-coated" peel ply's on the market which are coated in release agents to aid removal. These almost always leave a trace/layer of release agent on the finished part and will need a thorough key and clean to ensure all traces are removed to get a good bond.
If in doubt, we always recommend full surface preparation prior to bonding.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|