I've just completed the first stage post laying on the carbon fibre sheet however on close inspection I don't think there is enough resin to withstand sanding down. should I apply another coat whilst the first coat is still tacky. (1 1/2 hrs ago)
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi Jeff,

Yes if you feel there is not enough resin, then apply another coat and try again.  The firm but tacky stage is ideal as you can apply the resin directly.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
JeffA
JeffA
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 4, Visits: 17
Great, thanks for the quick reply.