Hello, I'm in the process of modifying my battery powered audio mixer in order to make it lighter, I was thinking of substituting the metal panels of the device with some carbon fibre sheets. In order to decide whether to do this or not I'd need to know how much weight I'd gain, more or less (I don't need anything ultra precise..). Is it possible to know the weight by square meter for the single sided 2mm and 1mm Sheets? Thanks
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The weights per square meter of our new Resin Infused High Strength Carbon Fibre Sheet are as follows:

1mm = 1.281kg
2mm = 2.401kg
3mm = 4.081kg

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search