By Attila Faravelli - 2/21/2017 11:55:40 PM
Hello, I'm in the process of modifying my battery powered audio mixer in order to make it lighter, I was thinking of substituting the metal panels of the device with some carbon fibre sheets. In order to decide whether to do this or not I'd need to know how much weight I'd gain, more or less (I don't need anything ultra precise..). Is it possible to know the weight by square meter for the single sided 2mm and 1mm Sheets? Thanks
|
By Warren (Staff) - 2/22/2017 12:46:57 PM
The weights per square meter of our new Resin Infused High Strength Carbon Fibre Sheet are as follows:
1mm = 1.281kg 2mm = 2.401kg 3mm = 4.081kg
|
|