Hi guys,

I'm a bit confused regarding all those release agents. Do I have to buy all of them:

- PVA
- Number 8 Wax
- Easy-Lease Chemical release

or one of them would do?

The surface on which I'm going to do a vacuum infusion would be one of these:

- Polypropylene sheet
- Polycarbonate sheet
- PVC sheet
- Plexiglass (perspex) sheet

It would be nice if Matt (staff) or someone else who works at EC could explain a bit more about those release agents and the materials I want to use them on.

Thank you
Reply
mannime
mannime
Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)Forum Guru (57 reputation)
Group: Forum Members
Posts: 7, Visits: 31
Hi Matt,

thank you very much for thorough explanation of each release agent.  So it seems that I will be ordering Easy-Lease.

Could you confirm that it will work ok with one of the mould surfaces below?

- Polypropylene sheet
- Polycarbonate sheet
- PVC sheet
- Plexiglass (perspex) sheet

I'm I right thinking that the first 2 materials would be the best followed by PVC and then perspex? Which would you choose personally?

I really appreciate your help.

Thank you,
Mani
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search