make_pr
make_pr
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 9,
Visits: 93
I want to place a part made with PX6 into a mould and use PX90 around the part to set around it. I have designed the part with features to hold onto the PX90. Will the PX90 adhere to the PX6 part if I rough the surface up or do I need to place some adhesive around the part to adhere it to the PX90 ?
Reply
Like
5
Warren (Staff)
Warren (Staff)
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Generally PU bonds to PU in cases like this, however it is not one I have tested personally.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search