By make_pr - 1/9/2017 11:51:55 AM
I want to place a part made with PX6 into a mould and use PX90 around the part to set around it. I have designed the part with features to hold onto the PX90. Will the PX90 adhere to the PX6 part if I rough the surface up or do I need to place some adhesive around the part to adhere it to the PX90 ?
|
By Warren (Staff) - 4/27/2017 9:06:42 AM
Generally PU bonds to PU in cases like this, however it is not one I have tested personally.
|
|