Hi everyone.

First off thanks to everyone on here. I've read a lot of interesting threads and have learnt a lot.

I've got a project going on right now where I need to cast multiples of a large piece. The volume of the pattern is 37ltrs which is around 41kg of resin with no filler.

I've worked out the split lines on the mould and I think these will work well given the shape. All surfaces have a draft of 6 degree's and any parallel sides are on the split lines. If anyone can take a quick look over the attached image and just make sure I haven't made any glaring errors.

My question is how to cast such a large piece. I'll be using ATH filler in a quantity of 1:1 ie. 1 part ATH to 1 part mixed resin.

  • Will this allow to mix a few batches of resin and pour this in to the mould before the whole thing sets?
  • What's the maximum safe amount of resin/ATH amount to mix in one container? Any idea on pot life?
  • What's the best choice of resin? EC sell xencast P6 which I plan if suitable.
  • Can I do an in-mould coating of pattern coat primer to provide a surface that will accept paint straight out of the mould?
Thanks for any help.
Attachments
Mould1.jpg (523 views, 111.00 KB)
Replies
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
50mm!! you're not building a submarine hull!!
Shinobiwan
Shinobiwan
Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)
Group: Forum Members
Posts: 14, Visits: 97
ChrisR (29/12/2016)
50mm!! you're not building a submarine hull!!


Overkill? OK well how best to add mass and thickness?
Edited 9 Years Ago by Shinobiwan
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
I think you need to post the dimensions of the thing including hole size etc (or pm of you don't want to make that public) if you want any specific advice.
Shinobiwan
Shinobiwan
Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)
Group: Forum Members
Posts: 14, Visits: 97
Dimensions are approx 800mm x 550mm x 185mm.

Really important question: What's the shrinkage like on Polyester, Vinylester and Epoxy laminating resins? With holes and critical parts fitting together during assembly the shrinkage really needs to be less than 1%.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Shinobiwan - 9 Years Ago
Fasta - 9 Years Ago
Shinobiwan - 9 Years Ago
Fasta - 9 Years Ago
Hanaldo - 9 Years Ago
ChrisR - 9 Years Ago
Shinobiwan - 9 Years Ago
Shinobiwan - 9 Years Ago
ChrisR - 9 Years Ago
Shinobiwan - 9 Years Ago
                 50mm!! you're not building a submarine hull!!
ChrisR - 9 Years Ago
Shinobiwan - 9 Years Ago
ChrisR - 9 Years Ago
Shinobiwan - 9 Years Ago
Shinobiwan - 9 Years Ago
ChrisR - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search