I'm planning to make this bracket with CF but don't have a lot of experience working with it and need advice. 
1) the radius of .5 in the ones with the ? mark. How small can I go? Thinking about using vacuum forming.
2) For the shape. I'm thinking about making a male in wood, lay the fabric on top and once is cure machining the contour. Is this a good idea?
3) What about the thread. Should I make a metal insert ?
Any advice would be welcome.
thanks
Attachments
carbon bracket.pdf (392 views, 171.00 KB)
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
How thick walls would you use to make the bracket out of aluminium?  Thats a good guideline.. same thickness in solid CF .. Then test, you may get away with a thin core, but for a structural bracket, the saving in weight is probably not worth the bother.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search