Weak vacuum


Author
Message
milgravis
milgravis
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 92
This is mi first post here. I,m new to composites, vacuum baging etc... Working on mi project and having some problems with vacuum. Pump is 3GSM bag is 1.6m long and 40cm. wide. I don`t have good vacuum, kinde of weak. Checked for ail leaks- thereis non. What the problem? Thanks in advance!
Replies
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
First, remove all pipework up to where you are measuring the vacuum and cap off/seal/turn valve off.
Turn pump on and check you can achieve full vacuum (or close to)

If you can - you've got a leak in the bag/pipework/mould
If you can't - check the oil level (if the pump uses oil), if the oil level is good, check with another vac gauge if you've got one, if still no vac then you're pump's likely bad
milgravis
milgravis
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 92
Thanks for reply! Today in the morning I think that I`ve found problem. Pump i brand new (first time in use) and no leaks in bagging or pipes, but i`ve realize what I did wrong, was very tired yesterday. I did extend plate on which I did vacuum bagging with another plate and I did not seal the jointBlush So in was sucking up the air from under threw this joint. Well it was very first experience in vacuum bagging........ 